Sodium Nickel Iron Manganese Oxide Cathode Sheet (NT03XX), Single-Sided, 5 pcs
Single-sided sodium nickel iron manganese oxide (NFM) cathode coated on aluminium foil, ready to punch for sodium-ion battery research. Evaluated in 1.0M NaClO4 in EC:DEC (1:1 vol%) with 5.0% FEC.
Product Specifications
Material: Sodium Nickel Iron Manganese Oxide
Sheet Size (cm): 10*10
Current Collector Thickness (μm): 12
Current Collector Areal Density (mg/cm²): 3.30
Coating Areal Density (mg/cm²): 8.0 (±2.0%)
Areal Capacity (mAh/cm²): 0.97
Active Material Specific Capacity (mAh/g): 127 (2.00 – 4.00 V)
Active Material Ratio (%): 95.5
Compaction Density (g/cc): 2.0–2.5 g/cc (Calendered)
Test Conditions (Room Temperature 25 °C): 0.1/0.1C, 2.0-4.0V
Shelf Life: 6 months (vacuum sealed storage), use within 1 month after opening
Initial Charge and Discharge Test Conditions
Temperature: 25°C
Charge: First, charge at a constant current of 0.1C to 4.0V, then charge at a constant voltage until the current drops below 0.02C.
Discharge: Discharge at a constant current of 0.1C to 2.0V.
Rate Performance Test Conditions
Temperature: 25°C
Charge: First, charge at a constant current of 0.5C to 4.0V, then charge at a constant voltage until the current drops below 0.02C.
Discharge: Discharge at constant current rates of 0.1C, 0.2C, 0.5C, 1C, 2C, and 3C to 2.0V.
Cycle Test Conditions
Temperature: 25°C
Charge: First, charge at a constant current of 0.5C to 4.0V, then charge at a constant voltage until the current drops below 0.02C.
Discharge: Discharge at a constant current of 1C to 2.0V.
Typical Uses
Electrode for sodium-ion half cells and full cells
Benchmarking sodium-ion electrolytes and cell hardware
Notes
If the electrode is not pre-calendered, calendering is recommended to achieve the specified compaction density.
The areal density should be calculated based on the actual mass of each punched electrode.
Prior to use, the electrodes should be vacuum dried at 105 °C for 4 hours before transfer into the glove box.
Since the electrodes are single-side-coated, calendering may cause curling issues. Batch-to-batch variations are within normal manufacturing tolerances.